ASTM A53 E tipo B laipsnio planas 80 vamzdžių matmenys

Oct 17, 2023

 

ASTM A53 E tipo B laipsnio planas 80 vamzdžių matmenys

 

NPS žymeklis DN žymuo Išorinis skersmuo Vidinis skersmuo Sienos storumas Nominalus svoris (masė) vienam ilgio vienetui
(mm) (mm) (mm) Lygus galas (kg/m) Sriegiai ir movos (kg/m
1/8″ 6 10.3 5.5 2.41 0.47 0.46
1/4″ 8 13.7 7.7 3.02 0.8 0.8
3/8″ 10 17.1 10.7 3.2 1.1 1.1
1/2″ 15 21.3 13.9 3.73 1.62 1.62
3/4″ 20 26.7 18.8 3.91 2.2 2.21
1″ 25 33.4 24.3 4.55 3.24 3.25
1-1/4″ 32 42.2 32.5 4.85 4.47 4.49
1-1/2″ 40 48.3 38.1 5.08 5.41 5.39
2″ 50 60.3 49.3 5.54 7.48 7.55
2-1/2″ 65 73 59 7.01 11.41 11.52
3″ 80 88.9 73.7 7.62 15.27 15.39
3-1/2″ 90 101.6 85.4 8.08 18.63 18.82
4″ 100 114.3 97.2 8.56 22.32 22.6
5″ 125 141.3 122.3 9.52 30.94 31.42
6″ 150 168.3 146.3 10.97 42.56 43.05
8″ 200 219.1 193.7 12.7 64.64 65.41

ASTM A53 Type E Grade B Schedule 80 Pipes

 

ASTM A53 Type E Grade B Schedule 80 Tube